Material:Mo1,MoLa,TZM
Composition:Mo1:≥99.95%
MoLa:Mo + La2O3(0.5%~1%)
TZM: Mo + 0.40~0.55%Ti + 0.06~0.12%Zr + 0.01~0.043% C
Size: Ф10~150X100~1500mm,customized
Density: ≥10.15g/cm3
Process: Powder metallurgy
Surface: Forged, Ground
Product characteristics:
-- High temperature resistance
-- High strength
-- Strong corrosion resistance ,
-- Long service life
Process flow:
Powder--Pressing--Sintering--Forging--Heat treatment--Deep processing--Surface treatment--Inspection--Finished products--Packing
Applications:
--Used in optical glass, thermal insulation materials, glass fiber and rare earth industry.